Hello, I added a layer of fiberglass over the combing lip, it realy wasn't that hard to do, just make sure to use bias cut strips of cloth and I formed the glass under the lip by using a length of 5/8 inch clear plastic hose with a string inside of it and just tied it around the lip to hold the glass in place until it dried. Kenny > Howdy All-
> I am finishing my coaming lip and know that trying to wrap glass around it
> is going to be a lesson in frustration. Can I just seal it with epoxy and
> finish with varnish? The fiberglass from the inside of the deck does wrap
> around and cover the vertical part of the coaming. I also filleted the
> vertical strips and covered them with fiberglass when I did the outside of
> the deck. I have made the lip from strips of ash and glued them in place
> with Cab-O-Sil thickened epoxy. So it is just the ash lip that is not
> covered with fiberglass.
> Thanks for your help.
> Rick S.
Messages In This Thread
- Fiberglass coaming lip?
Rick S. -- 3/27/1999, 1:05 am- Re: Fiberglass coaming lip?
Kenneth Paul -- 3/27/1999, 11:28 am- Re: Fiberglass coaming lip?
Peter A Sarnosky -- 3/27/1999, 8:27 am - Re: Fiberglass coaming lip?
- Re: Fiberglass coaming lip?