Ditto to using the 207 for clear coating. It's MUCH better for anything that you're going to "bright finish." Note of caution: Be certain not to use the correct metering pumps. As I recall, the 207 uses a 3:1 ration of resin to hardner rather than the 5:1 used by the 205/206....
I used the 205/206 on my first boat and got a few "cloudy" patches here and there (mostly noticeably by me). Some of the cloudiness can be attributed to my "newbie" technique and initally using a foam brush.
Good luck.
Messages In This Thread
- West System Hardeners
Dave Seales -- 3/26/2001, 6:49 am- Re: West System Hardeners
Stan Snapp -- 3/26/2001, 11:57 am- Re: West System Hardeners
Byron -- 3/26/2001, 11:46 am- Re: West System Hardeners
Sam Mcfadden -- 3/26/2001, 11:02 am- Re: West System Hardeners
Dave Seales -- 3/26/2001, 12:47 pm- Hardeners
Sam McFadden -- 3/26/2001, 1:42 pm- Re: Hardeners
Stan Snapp -- 3/27/2001, 1:36 am
- Re: Hardeners
- Hardeners
- Re: West System Hardeners
- Re: West System Hardeners