: I'm up to the stage where I glass, I've had a couple of different reading sources that approach the process differently, Nick's does a sealer coat then glassing and others go right to glassing what's the difference. What do I get to thion out the MAS system that I got with Nick's kit? Also any tips on heating a workshop in Alaska? it's my garage here in Sitka, 28X14 with 11' cieling, it's warm enough to work in, but outside it's always 40's and dampuntil summer!
: I guess I'll have to get a thermometer to accurately measure the heat ands maybe a cieling fan to keep the heat from going upstairs?
I have recently been skipping the seal coat. The MAS
Epoxy is thin enough that it will soak right through
the glass and get sucked up by the wood without any
problem. You do not need to thin MAS epoxy.
Nick
Messages In This Thread
- glassing
Mike Mindiola -- 2/20/1998, 5:02 pm- Re: glassing
Mark Kanzler -- 2/20/1998, 5:02 pm- Re: glassing
Michael Vermouth -- 10/31/1997, 9:27 am- Re: glassing
Rob -- 10/31/1997, 9:45 am- Re: cold barn
Rob Herbert -- 10/31/1997, 9:44 am- Re: cold barn
Nick -- 10/31/1997, 9:44 am
- Re: glassing
Nick -- 10/31/1997, 9:43 am- Re: glassing
michael mindiola -- 10/31/1997, 9:29 am
- Re: glassing
- Re: glassing