By:Oliver L
Date: 4/14/2006, 2:41 pm
In Response To: Re: Epoxy: I bought the WS 205 hardener.... (Nick Schade - Guillemot Kayaks)

: For gluing 205 is the good stuff. If you want to wet out glass and have it
: stay clear, 207 is the appropriate hardener from West Systems.

So basically 205 for mixing filler, gluing stems and coaming. 207 for glassing. At what temperature should my shop be during this process?