Material: glass two layer w/o bubbles
By:LeeG
Date: 4/22/2002, 9:10 am
Date: 4/22/2002, 9:10 am
just looking for advice on the best way to reliably get two layers of 4oz glss down without bubbles developing. I did two layers of 4oz, one after the other partially cured and got tiny bubbles that show the variation in the tension of the fibers, not exactly wrinkles but those little 1/2" waves that seem to be a part of the cloth, sometimes it's more noticable than others. I wonder if I squeegeed too much on the second one. This isn't outgassing.