This is a little bit off subject, but I'll ask anyway. I don't think I'll have enough MAS epoxy to do the fill coats on my yak, but I have enough to do all the fiberglassing. I have a supply of WEST that I can use, not a lot, but at least half a gallon. Is it OK to use WEST as a filler if I wait a while and scrub, then sand very lightly to create a mech bond? I have a while to think about it, but thought I would ask. If need be, I can buy more MAS epoxy.

Messages In This Thread

Epoxy: wet out with MAS, filled with Sys 3...bad mix.
Bill Cruz -- 12/5/2003, 10:45 pm
Re: Epoxy: wet out with MAS, filled with Sys 3...b
hoz -- 12/6/2003, 9:24 am
Re: Epoxy: wet out with MAS, filled with Sys 3...b
Bill Cruz -- 12/7/2003, 2:40 pm
Re: Epoxy: wet out with MAS, filled with Sys 3...b
hoz -- 12/7/2003, 5:10 pm
Just curious,
Bill Cruz -- 12/8/2003, 1:38 am
Re: Just curious,
hoz -- 12/8/2003, 6:33 am
"Mr. Hoz,"
Bill Cruz -- 12/8/2003, 3:40 pm
Re: Epoxy: wet out with MAS, filled with Sys 3...b
Chuck -- 12/5/2003, 11:03 pm
Two brands of Epoxy...same project?
Bill Cruz -- 12/6/2003, 9:25 am
Well, maybe.
Paul G. Jacobson -- 12/5/2003, 11:45 pm