Date: 12/8/2003, 3:40 pm
: I let it cure to the "green" stage before applying the second coat.
: Still tacky, not fully cured. That way the second coat can adhere with a
: chemical bond.
Hoz,
Hey, I hope I'm not offending you by not heading this, "Mr. Hoz,". Good strategy here. I'm pretty sure given our seperate results, that the cold weather had much to do with the failure I had glassing the spray skirt lip of my current project. I think the fact that I was using two seperate brands of epoxy and harderner, one on top of the other "without any curing time allowed", also contributed. It's all sanding dust now anyway. I seal coated the surfaces prior to glassing, which I hope to get done tonight. Thanks mucho for your input here!!!
Bill
Messages In This Thread
- Epoxy: wet out with MAS, filled with Sys 3...bad mix.
Bill Cruz -- 12/5/2003, 10:45 pm- Re: Epoxy: wet out with MAS, filled with Sys 3...b
hoz -- 12/6/2003, 9:24 am- Re: Epoxy: wet out with MAS, filled with Sys 3...b
Bill Cruz -- 12/7/2003, 2:40 pm- Re: Epoxy: wet out with MAS, filled with Sys 3...b
hoz -- 12/7/2003, 5:10 pm- Just curious,
Bill Cruz -- 12/8/2003, 1:38 am- Re: Just curious,
hoz -- 12/8/2003, 6:33 am- "Mr. Hoz,"
Bill Cruz -- 12/8/2003, 3:40 pm
- "Mr. Hoz,"
- Re: Just curious,
- Just curious,
- Re: Epoxy: wet out with MAS, filled with Sys 3...b
- Re: Epoxy: wet out with MAS, filled with Sys 3...b
Chuck -- 12/5/2003, 11:03 pm- Two brands of Epoxy...same project?
Bill Cruz -- 12/6/2003, 9:25 am- Well, maybe.
Paul G. Jacobson -- 12/5/2003, 11:45 pm - Well, maybe.
- Re: Epoxy: wet out with MAS, filled with Sys 3...b
- Re: Epoxy: wet out with MAS, filled with Sys 3...b