Date: 4/3/2008, 3:39 pm
: Ok, should restate this anyway, the other reason for more than 4 coats is you
: don't gain enough UV resistance that way, the film thickness is just too
: thin. So takes multiple coats, though you lose a fair portion of that with
: sanding.
: Of course I'm used to varnishing boats that sit for a season in the sun
: rather than a few hours, so for them the UV resistance is of more
: importance. Last boat I did had 14 coats and used as I remember around 24
: quarts of varnish.
: Bill H.
For god's sake, please tell me that was a yacht that you were working on. Or maybe you're still in the April fools mode. With the what I just popped for a qt. of Pettit Flagship, I'll need a second mortgage just to finish my boats!
Todd
Messages In This Thread
- Material: varnishing
gilles moreau -- 4/2/2008, 8:14 pm- Re: Material: varnishing
Bill Hamm -- 4/3/2008, 3:23 pm- Re: Material: varnishing
Bryan Hansel -- 4/3/2008, 8:50 am- Re: Material: varnishing
Bill Hamm -- 4/3/2008, 12:39 am- Re: Material: varnishing
Glen Smith -- 4/3/2008, 9:00 am- Re: Material: varnishing
Bill Hamm -- 4/3/2008, 3:18 pm- Re: Material: varnishing
Todd Sullivan -- 4/3/2008, 3:39 pm- Re: Material: varnishing
Bill Hamm -- 4/4/2008, 10:52 am- Re: Material: varnishing
Todd Sullivan -- 4/4/2008, 11:39 am- Re: Material: varnishing
Bill Hamm -- 4/4/2008, 4:04 pm
- Re: Material: varnishing
- Re: Material: varnishing
- Re: Material: varnishing
- Re: Material: varnishing
- Re: Material: varnishing
- Re: Material: varnishing
Glen Smith -- 4/2/2008, 8:41 pm - Re: Material: varnishing
- Re: Material: varnishing