Re: Skin-on-Frame: coaming bending advice
By:Kudzu
Date: 5/28/2009, 11:22 pm
In Response To: Re: Skin-on-Frame: coaming bending advice (Ken Blanton)

3 or 4 mm(?) Okume. Can't remember which it is. It bends very well. A little heat and it bend tight bends.

Messages In This Thread

Skin-on-Frame: coaming bending advice
Michael -- 5/28/2009, 1:02 pm
Re: Skin-on-Frame: coaming bending advice
Michael -- 5/29/2009, 12:03 am
Re: Skin-on-Frame: coaming bending advice
Brian Nystrom -- 5/29/2009, 12:09 pm
Re: Skin-on-Frame: coaming bending advice
Bill Hamm -- 5/29/2009, 2:07 pm
Re: Skin-on-Frame: coaming bending advice
Michael -- 5/29/2009, 2:56 pm
Re: Skin-on-Frame: coaming bending advice
Brian Lemin -- 5/29/2009, 9:25 am
Re: Skin-on-Frame: coaming bending advice
Michael -- 5/29/2009, 12:31 pm
Re: Skin-on-Frame: coaming bending advice
Bill Hamm -- 5/28/2009, 3:28 pm
Re: Skin-on-Frame: coaming bending advice
Brian Lemin -- 5/29/2009, 10:24 pm
Re: Skin-on-Frame: coaming bending advice
Mike Savage -- 5/30/2009, 6:39 am
Re: Skin-on-Frame: coaming bending advice
Brian Lemin -- 5/31/2009, 12:40 am
Re: Skin-on-Frame: coaming bending advice
Bill Hamm -- 5/30/2009, 11:06 am
Re: Skin-on-Frame: coaming bending advice
Kudzu -- 5/28/2009, 1:11 pm
Re: Skin-on-Frame: coaming bending advice
Ken Blanton -- 5/28/2009, 3:55 pm
Re: Skin-on-Frame: coaming bending advice
Kudzu -- 5/28/2009, 11:22 pm