: 10-micron it is! I'll order it soon, as I have no clue what kind of lead time
: i might be looking at. From earlier posts I've read through, I was
: thinking of going for a 15% HBN and 5% Colloidal Silica mixture.
: Impressive to hear that it holds up well to ice. I may use it when I
: refinish the below waterline coating on my Shearwater Hull. It'd be cool
: to not have to worry about being around ice once parts of the Chesapeake
: freeze over-
I'd agree with the 5% silica but I'd add as much HBN as it'll take, within reason and still be spreadable. 15-20% is about all it'll take, if it's like the graphite it floats in the resin, hard to get it mixed.
Bill H.
Messages In This Thread
- Material: HBN source in the US *LINK*
Johnathan Akers -- 10/20/2009, 2:05 pm- Re: Material: HBN source in the US
Robert N Pruden -- 10/20/2009, 10:10 pm- Re: Material: HBN source in the US
Johnathan Akers -- 10/21/2009, 12:41 am- Re: Material: HBN source in the US
Bill Hamm -- 10/22/2009, 3:00 am- Re: Material: HBN source in the US
Robert N Pruden -- 10/21/2009, 9:41 am- Re: Material: HBN source in the US
Johnathan Akers -- 10/21/2009, 10:46 pm
- Re: Material: HBN source in the US
- Re: Material: HBN source in the US
- Re: Material: HBN
Paul G. Jacobson -- 10/20/2009, 9:27 pm- Re: Material: HBN
Johnathan Akers -- 10/21/2009, 12:37 am
- Re: Material: HBN source in the US
- Re: Material: HBN source in the US