: Question - My warehouse is ice cold (around 40 degrees) and no way
: I am paying to heat it. Would it work just as well to peg and
: lash it and skip the epoxy/glue all together? I am talking
: chines, keel, and gunwales. (no warm temps in sight)
Lashing is IMHO the idea way. I have built 3 or 4 now and I lash all mine with no glue in frame at all. Get some waxed artificial sinew and just lash them tight. I know a lot of people use different things to lash with and all of them will work. But the beauty of waxed sinew is when you let off tension the joint doesn't loosed up. It sticks to itself and makes 'tying off' much easier. After doing a few I am a convert! All my boats will be lashed from now one
I made a video on lashing. www.kudzucraft.com/video/lashing.php
Messages In This Thread
- Skin-on-Frame: Wasted Days and Wasted Nights
danp -- 2/13/2010, 1:20 am- Re: Skin-on-Frame: Wasted Days and Wasted Nights
brian scarborough -- 2/14/2010, 9:04 pm- Re: Skin-on-Frame: Wasted Days and Wasted Nights
Scott Shurlow -- 2/14/2010, 4:18 pm- Re: Skin-on-Frame: Wasted Days and Wasted Nights
Kudzu -- 2/13/2010, 8:46 am- Re: Skin-on-Frame: Wasted Days and Wasted Nights
Gary Kvasnicka -- 2/13/2010, 8:46 am- Re: Skin-on-Frame: Wasted Days and Wasted Nights *PIC*
Dave Gentry -- 2/13/2010, 3:56 am - Re: Skin-on-Frame: Wasted Days and Wasted Nights
- Re: Skin-on-Frame: Wasted Days and Wasted Nights