Date: 5/25/2010, 9:36 pm
A heat gun should really help with the pulling off with pliers part.
Brian
: If it won't take any more resin and just stays white, then yeah,
: looks like you get to sand it off. Might try pulling it off with
: pliers (catfish skinning pliers?), try scrapers, try a wire
: wheel in a drill, try anything and everything that sounds like
: it might work. Use caution when experimenting, of course; the
: idea is to save retro time, not add hours to the project.
: I once got about halfway through glassing out a deck and had an
: emergency call me away, couldn't get back to it for 24 hours.
: The "wet edge" I left was well defined, and the next
: day I simply took up where I left off, and it worked out well
: except you could see where the break in the action had occurred.
: But lo and behold, the demarcation faded, then vanished
: altogether in a couple days. That was on my Cormorant, in '04,
: and I'm still paddling that sweetheart.
: Good luck with yours, and let us know what happens....?
Messages In This Thread
- Strip: glassing *PIC*
buck biscuit -- 5/25/2010, 6:59 pm- Re: Strip: glassing
Dave -- 5/31/2010, 10:13 am- Re: Strip: glassing
Bill Hamm -- 6/3/2010, 2:38 pm
- Re: Strip: glassing
Kurt Maurer -- 5/25/2010, 7:08 pm- Re: Strip: glassing
Brian Scarborough -- 5/25/2010, 9:36 pm- Re: Strip: glassing
Allan -- 5/25/2010, 10:50 pm- Re: Strip: glassing
Mike Hanks -- 5/25/2010, 10:28 pm - Re: Strip: glassing
- Re: Strip: glassing
- Re: Strip: glassing
- Re: Strip: glassing