Date: 2/7/2011, 6:40 pm
: There is no stsandard calculation for a "14 foot kayak".
: It depends on the type of construction.Glass on seams only? Glass
: on hull? Outside? Inside? Glass on deck? What weight of glass?
: Have you ever done anything like this before? Do you know the
: difference between an exposed weave lamination and a filled
: lamination?
: You didn't give us the name of your design. If you are designing a
: one-off you will probably need twice as much.
I am a first time Kayak builder but not first time using glass. I plan on doing both inside and out of the hull and posiblly two layers on the hull bottom. I live in Arkansas and will be in small streams and rivers or lakes. The deck I was not going to glass but just use spar varnish.
Messages In This Thread
- S&G: Resin and hardner.
mlanford -- 2/7/2011, 3:01 pm- Re: S&G: Resin and hardner.
MattD -- 2/7/2011, 5:56 pm- Re: S&G: Resin and hardner.
Charlie -- 2/7/2011, 6:13 pm- Re: S&G: Resin and hardner.
mlanford -- 2/7/2011, 6:40 pm- Re: S&G: Resin and hardner.
mlanford -- 2/7/2011, 6:44 pm- Re: S&G: Resin and hardner.
Bill Hamm -- 2/8/2011, 12:25 am
- Re: S&G: Resin and hardner.
- nominal gallon is best pricewise
Paul G. Jacobson -- 2/7/2011, 11:36 pm- Re: S&G: Resin and hardner.
Bill Hamm -- 2/8/2011, 12:21 am- Re: S&G: Resin and hardner.
Fred Gasper -- 2/8/2011, 7:33 am - Re: S&G: Resin and hardner.
- Re: S&G: Resin and hardner.