Hey everyone,
Had been off to NW GA and had plenty time to think and ponder the next few steps of the Yost SeaTour build. I have read about laminating a coaming, and Kudzu's technique instructional is very handy.

Using the Yost 16x30 inside dimensions, can I build one with some leftover WRC I have on hand? I got a 16'x.75"x1.5" and another 16'x.75"x1" that I can have ripped somewhere into 1/8" strips.

Most suggest the coaming be about 3/8" wide and 1.5" deep with a lip that I am not sure what dimensions it should be. Can it be only 1" deep as suggested (by Brian Nystrom???) in a thread somewhere ( I wanna roll on this thing)?

Oh and uuhhh... if the coaming is sewn in, how then does the fabric around the coaming get coated later on???
Thanks as always.

Messages In This Thread

Skin-on-Frame: Laminated Coaming with WRC
QayaqGeek/Tavo -- 7/11/2011, 3:45 pm
Re: Skin-on-Frame: Laminated Coaming with WRC
Bill Hamm -- 7/12/2011, 1:42 am
Re: Skin-on-Frame: Laminated Coaming with WRC
Jeff Horton -- 7/12/2011, 7:40 am
Laminated Coaming
Jay Babina -- 7/12/2011, 8:00 am
Re: Laminated Coaming
Jeff Horton -- 7/12/2011, 12:32 pm
Re: Laminated Coaming
dave g -- 7/12/2011, 8:57 pm
Re: Laminated Coaming
Jeff Horton -- 7/12/2011, 9:20 pm
Re: Laminated Coaming
Bill Hamm -- 7/13/2011, 7:48 am
Re: Laminated Coaming
Bill Hamm -- 7/13/2011, 7:47 am
Re: Skin-on-Frame: Laminated Coaming with WRC
Wayne One (wwfloyd) -- 7/12/2011, 8:12 am
Re: Skin-on-Frame: Laminated Coaming with WRC
QayaqGeek/Tavo -- 7/13/2011, 4:11 pm