: Really dark wood decks left in the sun can get pretty hot, hot
: enough to cause problems with the glue softening.

: Bill H.

I have heard that postulated, but I have seen photos of what people claim are the results, and when I forwarded them to West they gave an alternate explanation that didn't involve softening glue. I have a dark hull, and it does get hot, but I've never had a problem.

m

Messages In This Thread

Material: titebond or titebond ll
greg root -- 3/7/2012, 10:08 am
Re: Material: titebond or titebond ll
Jim Looker -- 3/7/2012, 12:30 pm
Re: Material: titebond or titebond ll
Kevin Greer -- 3/7/2012, 3:43 pm
Re: Material: titebond or titebond ll
ancient kayaker -- 3/7/2012, 10:07 pm
Re: Material: titebond or titebond ll
Mike Bielski -- 3/7/2012, 8:23 pm
Re: Material: titebond or titebond ll
Bill Hamm -- 3/8/2012, 2:11 am
Re: Material: titebond or titebond ll
Mike Bielski -- 3/8/2012, 10:45 am
Re: Material: titebond or titebond ll
Will N 2 go -- 3/8/2012, 10:28 pm
Re: Material: titebond or titebond ll
Mike Bielski -- 3/9/2012, 1:06 am