: I started working on the Maroske-type fittings for my boat tonight.
: Instead of using glass and epoxy, I used a glass reinforced
: resin mixture. Seems to work really well - and very easy to do.

: Here's a link to my blog entry if anybody's interested:

:
: http://justyakkin2.blogspot.ca/2012/03/black-pearl-project-variation-on.html

: Cheers,
: Sean

Sean,
If the Bondo hair is anything like Fiberall the bond will fail. I once used Fiberall to get my footbraces installed for a trip and they failed. Might be worth a test. My rule of thumb now is that expoxy will bond to polyester but polyester will not bond to epoxy.
Best,
Reg

Messages In This Thread

Material: Maroske fittings - a variation *PIC*
Sean Dawe -- 3/21/2012, 9:57 pm
Re: Material: Maroske fittings - a variation
Stephen Troy -- 3/22/2012, 10:04 pm
Re: Material: Maroske fittings - a variation
Sean Dawe -- 3/22/2012, 10:17 pm
Re: Material: Maroske fittings - a variation
Reg Lake -- 3/23/2012, 2:50 pm
Re: Material: Maroske fittings - a variation
Sean Dawe -- 3/23/2012, 4:52 pm
Re: Material: Maroske fittings - a variation
george jung -- 3/25/2012, 12:10 pm
Re: Material: Maroske fittings - a variation
John Abercrombie -- 3/25/2012, 1:32 pm
Re: Material: Maroske fittings - a variation
Sean Dawe -- 3/27/2012, 9:05 am
Re: Material: Maroske fittings - a variation
John Abercrombie -- 3/27/2012, 1:07 pm