Date: 8/17/2012, 4:43 pm
: Guys I have finished the glass work on my Night Heron and now it's
: time for the big V. I need some guidance as to what varnish to
: use. I was not aware that different marine grade varnishes have
: different degrees of UV protection in them. With at least 6
: coats of varnish to be applied I have to believe that a gallon
: is the smartest way to go.
: Any ideas on what, where and how much I will need?
You won't need a gallon. I had some left over after putting five coats on a double. There is probably no chance of consensus on what brand to use. i started with Epiphanes but gave up because it is too hard to get where I live. Now I use Interlux Schooner and it seems fine.
Ric
Messages In This Thread
- Material: Marine grade spar varnish?????
Chris Wynne -- 8/17/2012, 4:19 pm- Re: Material: Marine grade spar varnish?????
Ric Moodie -- 8/17/2012, 4:43 pm- Re: Material: Marine grade spar varnish?????
Chris -- 8/17/2012, 5:21 pm- Re: Material: Marine grade spar varnish?????
Ric Moodie -- 8/17/2012, 6:33 pm- Re: Material: Marine grade spar varnish?????
Jeff Horton -- 8/19/2012, 5:44 pm
- Re: Material: Marine grade spar varnish?????
- Re: Material: Marine grade spar varnish?????
- Re: Material: Marine grade spar varnish????? *PIC*
robert l -- 8/18/2012, 12:26 am- Re: Material: Marine grade spar varnish?????
Randy Echtinaw -- 8/18/2012, 10:26 am- Re: Material: Marine grade spar varnish?????
John Abercrombie -- 8/18/2012, 4:24 pm
- Re: Material: Marine grade spar varnish?????
- Why 6 coats?
Jay Babina -- 8/18/2012, 12:43 pm- Re: Why 6 coats?
Sodbuster------WebKitFormBoundary6pLaVD9X7Zfw4+Pi- -- 8/18/2012, 2:16 pm- Re: Why 6 coats?
Etienne Muller -- 8/18/2012, 3:23 pm- Re: Why 6 coats?
John Abercrombie -- 8/18/2012, 4:25 pm- Re: Why 6 coats?
ancient kayaker -- 8/18/2012, 10:46 pm- Re: Why 6 coats?
Etienne Muller -- 8/19/2012, 6:09 am- Re: Why 6 coats?
ancient kayaker -- 8/19/2012, 8:23 am
- Re: Why 6 coats?
- Re: Why 6 coats?
- Re: Why 6 coats?
Dan Caouette -- 8/19/2012, 8:42 am- Re: Why 6 coats?
Etienne Muller -- 8/19/2012, 8:55 am- Re: Why 6 coats?
Dan Caouette -- 8/19/2012, 10:34 am- Re: Why 6 coats?
Bill Hamm -- 8/20/2012, 2:14 am
- Re: Why 6 coats?
- Re: Why 6 coats?
- Re: Why 6 coats?
Robert l -- 8/20/2012, 7:24 pm- Re: Why 6 coats?
Jim Schaffer -- 8/21/2012, 7:53 pm- Re: Why 6 coats?
John Abercrombie -- 8/21/2012, 8:14 pm- Re: Why 6 coats?
Jim Schaffer -- 8/21/2012, 8:37 pm- Re: Why 6 coats?
Marc Upchurch -- 8/21/2012, 10:50 pm- Re: Why 6 coats?
Bill Hamm -- 8/22/2012, 12:53 am- Re: Why 6 coats?
Bill Hamm -- 8/22/2012, 12:55 am- Re: Why 6 coats?
Etienne Muller -- 8/22/2012, 4:01 am- Re: Why 6 coats?
Marc Upchurch -- 8/22/2012, 8:25 pm- Re: Why 6 coats?
Etienne Muller -- 8/23/2012, 3:54 am
- Re: Why 6 coats?
Rod Tait (Orca Boats) -- 8/22/2012, 8:51 pm- Re: Why 6 coats?
John Abercrombie -- 8/22/2012, 8:56 pm- Re: Why 6 coats?
Rod Tait (Orca Boats) -- 8/22/2012, 9:15 pm- Re: Why 6 coats?
Bill Hamm -- 8/23/2012, 6:14 am- Re: Why 6 coats?
Etienne Muller -- 8/23/2012, 11:41 am
- Re: Why 6 coats?
- Re: Why 6 coats?
- Re: Why 6 coats?
- Re: Why 6 coats?
- Re: Why 6 coats?
- Re: Why 6 coats?
John Abercrombie -- 8/22/2012, 2:39 am- Re: Why 6 coats?
Jim Schaffer -- 8/22/2012, 3:11 pm
- Re: Why 6 coats?
- Re: Why 6 coats?
- Re: Why 6 coats?
- Re: Why 6 coats?
ancient kayaker -- 8/22/2012, 1:47 pm- Re: Why 6 coats?
Robert l -- 8/22/2012, 1:59 pm
- Re: Why 6 coats?
- Re: Why 6 coats?
- Re: Material: Marine grade spar varnish?????
- Re: Material: Marine grade spar varnish?????