Date: 7/31/2013, 11:31 am
Hi.
It has been about a year sense I glassed the top of my first strip build and I am just now getting around to starting on the inside. I did not trim the excess glass and epoxy at the sheer line so it is hanging down with visqen and tape separating it from the bottom half. The problem I am having is when I try and cut it at the shear line it is de laminating (White crack blister looking) for 1/4” to 1/2” up on the first strip when their is any out word force on the glass. i.e. When you push a razor knife in and then pull it out.
What should I do?
I am thinking I will need to sand threw the glass to the wood before I glass the sheer line seam.
I will try and post pix later.
Messages In This Thread
- Strip: Delamination at sheer line
Jaoson R. Moore -- 7/31/2013, 11:31 am- Re: Strip: Delamination at sheer line
john Messinger -- 7/31/2013, 12:12 pm- Re: Strip: Delamination at sheer line
Etienne Muller -- 7/31/2013, 12:18 pm
- Re: Strip: Delamination at sheer line
Allan -- 7/31/2013, 5:15 pm- Re: Strip: Delamination at sheer line
Bill Hamm -- 8/1/2013, 12:48 am- Re: Strip: Delamination at sheer line *PIC*
Jaoson R. Moore -- 8/16/2013, 5:23 pm - Re: Strip: Delamination at sheer line
- Re: Strip: Delamination at sheer line